A controlled expansion alloy, consisting of 51% Nickel, balance Iron, used in a wide variety of electronic applications, especially for glass seals. Alloy 52 is a nickel iron alloy whose coefficient of expansion closely mirrors soft glass. Applications for this product include magnetic reed switches and seals that need controlled linear expansion to approximately 525 °C.

Alloy 52 Basic Chemical Composition (Weight %)

Ni  50.50
Cr  0.10 max
Mn  0.60 max
Si  0.30 max
C  0.05 max
Al  0.10 max
Mg  0.50 max
P  0.025 max
S  0.025 max
Fe  Balance  

Typical Mechanical Properties

Alloy 52

Annealed

As Rolled

Ultimate Tensile Strength (PSI)

75,000

130,000

Yield Strength (PSI)

 30,000

125,000 

Elongation

30%

1%

Modulus of Elasticity (PSI)

24 x 10e6

Poisson's Ratio

0.29

Typical Physical Properties

Density                         0.300 lbs/cu in

Melting Point                    1425° C

Electrical Resistivity @ RT       43 Microhm-cm

Temp. Coefficient Resistivity      2900 PPM/°C 

(20 to 100° C)

Thermal Expansion Coefficient   10.0 x 10e-6/°C

(30 to 400° C)   

Applications

Glass to metal seals for electronic tubes, automotive and industrial lamps, and specialty hermetic devices.

Available Forms

Alloy 52 is available in Strip, Sheet, Plate and Wire.


  • Previous:
  • Next:

  • The use and maintain of the sawblade

    ◎ The carbide tip of sawblade is very sharp, so process of using must be prevent the carbide tip.

    ◎ PeriodicaI cleaning and support the machine,the spindle’s running tolerance must be less than h7.

    ◎ The flanges must be parallel to each other,must be of the same diameter 1/3 of the sawblade’s diameter(formuIti—rip saw blade is 1/2.

    ◎ When instaIIion the sawbIade,it shaII be 5-6 teeth higher than board surface.

    ◎ Before operation,check the firmly of the sawblade,be sure nobody in front of the machine. Do not feed of operation check whether the machine is good for operaiton. Periodical check the function of the machine,the certicaI jump is less than ±0.02MM,and the flap is less than ±0.01.

    ◎ After continuous use,must be removed and cleaning the sawblade,get rid of the resin and sawdust of the sawblade of both sides.Other wise it would beinfluence the effect of using the sawblade.

    ◎ Deposit of the sawblade,must not be layer the sawblade,it is putted in the originaI package inside.

    The renovate of the sawbIade

    ◎ The renovate of the carbide sawblade While it no longer sharpen and the horizontaI piece coarseaess. The power of using sawblade machine obviously Increase. When process materiaI,the materiaI appearred burst. The carbide tip exhaust more than 0.02MM.

    ◎ For the renovate the sawblade,it shouId be grinding by the a formal company, so be sure the quality of the sawblade after renovating.